SINFT® Knitted Wire Mesh is available from stock in a wide range of metal wire mesh. stainless steel is a popular option for demister pad material, as it provides an effective balance of strength and corrosion resistance. Known for its ability to withstand harsh environments and extreme working conditions, Knitted Wire Mesh is specifically engineered to endure all the challenges faced by oil and gas industries.
Need a knitted wire mesh demister pad material? Other alloys are metal available upon request. Visit our specialty alloys page for additional information about our copper and nickel alloys, such as Monel mesh, Inconel msh, 20Cb3, Titanium alloy wire mesh
As an added benefit, SINFTFILTER is located in the world's largest metal wire mesh industrial zone, and we are also a mature filter manufacturer with 17 years of experience. Our mature production experience in filters, DEMISTER, and filter wire mesh provides us with a mature industrial supply chain, enabling us to offer unparalleled price advantages and quality assurance to our customers.
Download a copy of our raw material guide for convenient referencing, and do not hesitate to contact us with any additional questions.
SUS 300 Series knitted wire mesh
SUS 304 (UNS: S30400) is a basic, austenitic stainless steel containing a minimum of 18% chromium and 8% nickel. This material meets the chemistry of the ASTM A580 specification.
Series Stainless 304L (UNS S30403) is a low carbon variation of Type 304 with a 0.03% maximum carbon content. This material meets the chemistry of the ASTM A580 specification.
Stainless 316 is an austenitic chromium-nickel-molybdenum stainless steel with good general corrosion resistance and improved pitting resistance. UNS S31600 – Cr: 16.0-18.0%, Ni: 10.0 – 14.0%, Mo: 2.0-3.0% with full chemistry to ASTM A580
The low carbon content in Stainless 316L is intended to minimize the occurrence of grain boundary carbide precipitation. UNS S31603 – C: 0.03% max, Cr: 16.0-18.0%, Ni: 10.0-14.0%, Mo: 2.0-3.0% with full chemistry to ASTM A580
Stainless 317L is a molybdenum bearing austenitic stainless steel with improved corrosion resistance over type 304/304L and type 316/316L stainless steel. UNS S31703 – C: 0.03%m max, Cr: 18.0-20.0%, Mo: 3.0-4.0% and Ni: 11.0-15.0% with full chemistry to ASTM A580
Stainless 321 is a titanium stabilized austenitic stainless steel commonly used for service in the temperature range of 1000°F (538°C) to 1600°F (870°C).UNS S32100 – Cr: 17.0-19.0%, Ni: 9.0-12.0%, Ti: 5xC min with full chemistry to ASTM A580
Stainless 347 is an austenitic stainless steel alloyed with columbium (niobium) offering an excellent resistance to intergranular corrosion. UNS S34700 – Cr: 17.0-19.0%, Ni: 9.0-13.0%, Cb: 10xC min with full chemistry to ASTM A580
Alloy |
C |
Mn |
Si |
P |
S |
Cr |
Ni |
Mo |
Cu |
Co |
Al |
Ti |
N |
Cb |
V |
304 |
0.08% max |
2.00% max |
1.00% max |
0.040% max |
0.030% max |
18.00- 20.00% |
8.00- 10.00% |
0.75% max |
0.75% max |
|
|
|
|
|
|
304L |
0.030% max |
1.25-2.00% max |
0.20-0.75 |
0.030% max |
0.015% max |
18.0-19.0% |
8.75-19.0% |
8.75-9.75% |
0.50% max |
0.50% max |
0.015% max |
|
0.050% max |
|
|
316 |
0.035-0.070% |
1.0-2.0% |
0.70% max |
0.040% max |
0.015% max |
16.5-18.0% |
10.50 – 12.0% |
2.0-3.0% |
0.50% max |
0.30% max |
0.010% max |
0.03% max |
0.060% max |
0.05% max |
|
316L |
0.03% max |
1.25-2.00% |
0.25-0.75% |
0.040% max |
0.030% max |
16.5-18.0% |
10.5-11.0% |
2.0-2.25% |
0.60% max |
|
|
|
0.070% max |
|
|
317L |
0.03%max |
2.0% max |
0.75% max |
0.045% max |
0.030% max |
18.0-20.0% |
11.0-15.0% |
3.0-4.0% |
0.50% max |
|
|
|
0.050% max |
|
|
321 |
0.020-0.060% |
1.25-2.00% |
0.40-0.80% |
0.030% max |
0.010% max |
17.0-19.0% |
9.0-11.0% |
0.60% max |
0.50% max |
0.50% max |
0.150% max |
5xC(C+N)-0.70% |
0.040% max |
|
|
347 |
0.040-0.060% |
2.00% max |
1.00% max |
0.040% max |
0.015% max |
17.0-19.0% |
9.0-12.0% |
0.50% max |
0.50% max |
|
|
|
0.060% max |
|
|